Physical Properties of Stainless steels
Designations Density Modulus of
elasticity
Mean coefficient of
thermal expansion
[10−6·K−1]
Thermal
Conductivity
Specific
Heat
Electrical
resistivity
EN
[]
AISI/ASTM at 20 °C
[kg/dm3]
at 20 °C
[GPa]
20 °C
200 °C
20 °C
400 °C
at 20 °C
[W/(m·K)]
at 20 °C
[J/(kg·K)]
at 20 °C
[(Ω·mm2)/m]
Austenitic stainless steels
1.4301 304 7,9 200 16,5 17,5 15 500 0,73
1.4401 316 8,0 200 16,5 17,5 15 500 0,75
Duplex stainless steels
1.4462 2205 7,8 200 13,5 14,0 (g) 15 500 0,80
1.4362 2304 7,8 200 13,5 14,0 (n) 15 500 0,80
1.4501   7,8 200 13,5 (n.r.) 15 500 0,80
Ferritic stainless steels
1.4512 409 7,7 220 11,0 12,0 25 460 0,60
1.4016 430 7,7 220 10,0 10,5 25 460 0,60
Martensitic stainless steels
1.4021 420 7,7 215 11,0 12,0 30 460 0,60
1.4418   7,7 200 10,8 11,6 15 430 0,80
Precipitation hardening stainless steels
1.4542 630 7,8 200 10,8 11,6 16 500 0,71